A building project is typically handled in a series of stages, each with its own manager. The goal is always to hand off each stage from one manager to the next without delays. But when moisture-sensitive flooring is involved, one part of the job can throw a wrench in the process: the concrete slab.
What’s Required for a Successful Flooring Installation?
For a flooring installation to be successful:
- The slab’s moisture and pH levels need to be within the acceptable range.
- The slab must be protected from outside moisture.
- The slab’s moisture level must be compatible with both the specified floor covering and the flooring adhesive.
- The potential for moisture emission from the slab must be addressed.
What Factors Delay a Slab’s Drying Time?
Many industry standards guide how a concrete slab is placed and dried, but the drying time for any slab is almost impossible to predict. The factors that affect drying time are unique to each installation. They include:
- The components of the original concrete mix
- 周囲の空気湿度
- 最終的なサービス条件
- 表面仕上げ
- How well the HVAC system is working
- 浮遊練習または再湿潤
When any of these factors change during the project, the concrete may need more time to dry. Delays in getting a properly dried slab can throw off the entire construction schedule.
スラブが乾くのを待つ方が良いのか、それともそのまま作業を進める方が良いのか?
Lost labor hours and added costs are two results of schedule interruptions on a construction project. But the alternative, pushing ahead despite the slab’s condition, risks flooring failure. A moisture-related flooring problem is a no-win situation for everyone involved, from contractors and construction managers to flooring installers, adhesive manufacturers, and facility owners. Experience shows that installing flooring before the slab’s moisture issues are resolved costs far more than waiting and getting it right the first time.
時計ではなくゴールに全員の視線
The ultimate goal of a construction project is an installed flooring system that stays problem-free for the long term.
When the construction schedule leaves no room to deal properly with moisture in the concrete, there’s a temptation to rush the project, and that invites flooring failure.
無料ダウンロード – コンクリートがなかなか乾かない4つの理由
スラブが完成したかどうかを知る方法
Some methods, such as desiccant drying and surface treatments, can help speed up drying. But how can the flooring contractor be sure the slab’s moisture level is compatible with the moisture-sensitive adhesive and flooring on the project?
正確に測定する relative humidity (RH) within the slab is the best way to know when the slab has dried enough.
Surface-only indicators of a slab’s moisture condition, such as calcium chloride testing, aren’t reliable, even though they have been widely used in the industry.
In-situ RH testing is better than surface-only testing because it reflects the RH conditions the slab will reach under an installed floor. With accurate knowledge of the slab’s RH, the general contractor and flooring installer will know whether to allow more drying time to meet the adhesive and flooring specifications, or to choose a different adhesive or flooring product that’s compatible with the slab’s current condition. RH testing gives everyone on the project the information they need to decide whether to wait or move on to the flooring installation.
ジェイソンは、幅広い業界で20年以上の営業および営業管理の経験を持ち、オリジナルのRapid RH®コンクリート水分試験器を含む様々な製品を市場に投入してきました。現在は、Wagner MetersでRapid RH®製品営業マネージャーを務めています。
最終更新日: 9 年 2026 月 XNUMX 日
歩道用のコンクリートを流し込んでくれました。気温が40度くらいでセメントが水っぽくて固まらなかったんです。暗くなってから帰ってしまいました。翌日また来て仕上げてもらえますか? 何度も「失敗した」って言ってました! 午前3時に出発したので、明日また来てデザインを入れてもらえるのは安心です。お願いできますか?
ジェリー:
コメントありがとうございます。現実的にそのような可能性があるとは聞いたことがありません。通常、コンクリートは適切な仕上げが不可能なほど硬化してしまいます。頑張ってください。
新築を建てる予定で、磨き仕上げのコンクリート床にしたいのですが、フロリダ州ネイプルズではスラブが乾くのに時間がかかり、ひび割れが増えるので、まずラミネートフローリングを敷くように建築業者に言われました。何かアドバイスはありますか?待ちたくないので、ひび割れはすぐに直したいと思っています。これは良い考えでしょうか?
ジュディス:
コメントありがとうございます。ラミネート加工を施してからコンクリートを研磨するという工程については、これまで聞いたことがありません。お住まいの地域でコンクリート研磨を専門に行っている会社にご相談されることをお勧めします。Googleで簡単に検索してみましたが、ネイプルズ周辺にいくつかあるようです。
よろしく、
ジェイソン
私の建築業者は、基礎工事の 15 時間後に 20 個の CMU パレットを基礎の上に積み込みました。
それは問題でしょうか、それとも速硬化セメントを使用しているのでしょうか?
ありがとうございました。
ボブ
ボブ:
質問ありがとうございます。でも、これは私が答えられる質問ではありません。頑張ってください。
ジェイソン